Here's the first GRP Dynamite fuse layed up in the new mould
It's epoxy resin with two layers of 4oz plain weave cloth all over and a third layer from about the C of G forward.
Hopefully it will come out of the mould nicely, will have to wait 'till monday to find out
and a view from the nose looking through the middle
It's epoxy resin with two layers of 4oz plain weave cloth all over and a third layer from about the C of G forward.
Hopefully it will come out of the mould nicely, will have to wait 'till monday to find out
and a view from the nose looking through the middle